Scaled Depth of Burial: Three Variants for Practical Blast Design
Technical Note — TN-2026-001
Author: Brent Buffham — Blasting Apps (blastingapps.com)
Date:
15 March 2026


Abstract

Scaled Depth of Burial (SDoB) is commonly used in the open cut mining industry to assess blast energy confinement and predict outcomes including flyrock, airblast, and fragmentation quality. The standard set of formulas treat the column above the explosive as a single entity, but in real world applications, blastholes often contain a mix of inert materials, not limited to solid stemming, air decks, and water columns — each providing fundamentally different levels of confinement.

This technical note proposes additional considerations to better assess SDoB. Utilising a three-variant framework for SDoB calculations — Geometric, Adjusted, and Ignored — this will provide Drill and Blast Engineers and Designers a clearer picture of effective confinement when non-solid materials are present above the charge.

Worked examples are provided using real blast designs from the Kirra blast design application.


1. Background

The Scaled Depth of Burial concept, by Chiappetta and Treleven (1997) and adopted via Tobin (2013), provides an empirical measure of blast energy confinement. It is defined as the ratio of stemming height to the explosive column length, scaled to a reference length of 10 hole diameters.

The standard SDoB formula is:

SDoB = D / W^(1/3)

Where:

  • D = distance from the surface to the centre of the explosive mass W (m)

  • W = mass of explosive within M hole diameters of the collar zone (kg)

  • M = scaling factor (number of hole diameters)

The scaling factor M is commonly cited as 10 hole diameters (Tobin, 2013; Chiappetta & Treleven, 1997). However, the M value is capped depending on hole diameter. For smaller blastholes (diameter <= 100 mm), M is limited to 8; for production-scale holes (diameter > 100 mm), M is limited to 10.

If the actual ratio of charge length to diameter is less than the limit, the actual value is used instead. The author's recollection is that the 8-diameter threshold came up in conversation with Cameron McKenzie (Blastechnology), though it was a long time ago and the original published source is uncertain. (McKenzie, C., personal communication, 2021.)

M = MIN(8, charge_length / diameter)   when hole diameter <= 100 mm
M = MIN(10, charge_length / diameter)  when hole diameter > 100 mm

The full SDoB formula, as corrected by McKenzie (2021), through personal email communications, uses two empirical constants (C1 = 0.0005, C2 = 0.00923):

SDoB = (St + (C1 x M x Dh_mm)) / (C2 x Dh_mm x (M x density)^(1/3))

Where:

  • St = stemming height (m)

  • M = capped scaling factor (as above)

  • Dh_mm = hole diameter in millimetres

  • density = explosive product density (g/cc)

  • C1 = 0.0005

  • C2 = 0.00923

Note: The question of how an air deck should be handled in this calculation discussed between the author and McKenzie in the same correspondence — this technical note proposes one possible framework for addressing that question.

The resulting SDoB value is typically classified into confinement categories:

SDoB < 0.60 ........... Under-confined
  → Cratering, excessive flyrock and airblast

SDoB 0.60 – 0.92 ...... Transitional
  → Moderate surface activity, potential flyrock

SDoB 0.92 – 1.40 ...... Controlled Energy
  → Good fragmentation and heave, acceptable airblast

SDoB > 1.40 ........... Over-confined
  → Reduced fragmentation, excessive vibration

Classification adapted from Chiappetta & Treleven (1997) via Tobin (2013).

However, the original formula assumes that the material above the charge is solid stemming. In real-world operations, the column above the explosive charge often includes air decks (intentional or from slumped stemming), water (from groundwater ingress or wet holes), or combinations of all three. These materials provide, and their coupling provide different levels of confinement, often significant, yet the standard SDoB calculation does not distinguish between them.


2. The Three-Variant Framework

To address this gap, the author proposes the use of three variants of SDoB, each suited to different analytical purposes.

2.1 SDoB(Geometric)

The full distance from the top of the charge to the collar, regardless of what material fills that space. This is a pure geometric measurement.

SDoB(GEO) = (Collar Depth - Top of Charge Depth) / L10d

The numerator is simply the total column length above the explosive, including stemming, air, water, or any combination thereof.

Use case: General blast design and QA checks where you want a quick geometric indicator of charge position relative to the free face. Useful for pattern compliance auditing.

2.2 SDoB(Adjusted)

The geometric distance is retained, but each segment of the column above the charge is weighted by a confinement coefficient that reflects its ability to resist gas venting and contain blast energy.

SDoB(ADJ) = SUM( αi x Li ) / L10d

Where:

  • Li = length of the i-th segment above the charge (m)

  • αi = confinement coefficient for the material in that segment (coefficients are undetermined at the writing of this paper and are estimates only)

  • The sum is taken over all n segments above the charge

Proposed default confinement coefficients (indeterminate — to be calibrated):

Solid stemming (aggregate/crushed rock)
  Symbol: α_stem   Proposed: 1.00   Range: 0.85 – 1.00
  → Full confinement; benchmark material

Drill cuttings (unsized)
  Symbol: α_cut    Proposed: 0.70   Range: 0.50 – 0.85
  → Reduced interlock vs sized aggregate

Water
  Symbol: α_water  Proposed: 0.50   Range: 0.30 – 0.70
  → Provides hydrostatic confinement but is easily displaced

Air
  Symbol: α_air    Proposed: 0.10   Range: 0.05 – 0.20
  → Low but non-zero confinement; see discussion below

A note on air confinement: It may be tempting to assign air a coefficient of zero, but this is physically incorrect. At detonation pressures, the air column is rapidly compressed. Under adiabatic compression (gamma = 1.4 for air), even modest compression ratios generate significant transient back-pressure. For example, a 100:1 compression ratio would produce approximately 63 MPa of resistance — far less than stemming's inertial resistance, but not insignificant. The air provides pressure-based resistance (compressibility, per Boyle's Law and the adiabatic gas law P2 = P1 x (V1/V2)^gamma) while stemming provides inertia-based resistance (mass). Air resistance is high initially, but drops rapidly once the column begins to vent, while stemming resistance is more sustained. For sealed air decks (stemming plug above and below the air column), the effective coefficient may be toward the upper end of the range as the trapped gas has nowhere to vent until the stemming plug fails.

IMPORTANT: All coefficients above are indeterminate at the time of writing. They are proposed starting points informed by the physics of confinement and the ground shock coupling factor concept from TM 5-855-1 (US Army, 1986), but they have not been derived from or validated against a published calibration study. They should be treated as initial assumptions for further investigation, not as established values. Site-specific calibration against airblast, flyrock, and vibration monitoring data is essential before relying on SDoB(ADJ) results for operational decisions.

Use case: Vibration and airblast prediction, flyrock clearance radius estimation, and any analysis where the actual effectiveness of confinement matters. This is the most physically representative variant.

2.3 SDoB(Ignored)

Only solid material (stemming, aggregate, drill cuttings) counts toward the burial depth. Air and water columns are completely excluded.

SDoB(IGN) = SUM( Li for solid segments only ) / L10d

All air and water segments contribute zero to the burial depth.

Use case: The most conservative assessment. Best suited for flyrock risk management, regulatory compliance, and exclusion zone calculations where the question is: "how much solid material is actually containing this charge down?"


3. Worked Examples from Kirra

The following examples use three blastholes designed in the Kirra blast design application, each representing a different column configuration. All holes use a nominal 251 mm (9⅞") diameter, giving L10d = 10 x 0.251 = 2.51 m.

3.1 Hole 201 — Stemming + Air Deck + ANFO

image[Figure 1: Hole 201 — Charging Summary]

Deck 1: INERT — Stemming .... 0.0 m to 3.5 m .... 3.5 m
Deck 2: INERT — Air ......... 3.5 m to 5.5 m .... 2.0 m
Deck 3: COUPLED — ANFO ...... 5.5 m to 13.8 m ... 8.3 m
Explosive mass: 292.4 kg

Calculations (using the full SDoB formula with M = 10 for 251 mm diameter):

SDoB(GEO)  = St=5.5m (all material above charge) → SDoB = 1.43  
           → Over-confined
SDoB(ADJ)  = St=3.7m (1.0 x 3.5 + 0.10 x 2.0) → SDoB = 1.05  
           → Controlled Energy
SDoB(IGN)  = St=3.5m (solid stemming only) → SDoB = 1.01  
           → Controlled Energy

In this case, SDoB(ADJ) and SDoB(IGN) are close but no longer identical because the air column contributes a small amount of confinement (α = 0.10) in the adjusted variant. The geometric variant overstates the confinement — it suggests the hole is at the boundary of over-confinement when the effective confinement is actually well within the controlled energy range.

Relying on SDoB(GEO) alone could lead to a false sense of security regarding flyrock risk, or conversely, could lead an engineer to unnecessarily reduce stemming.

3.2 Hole 202 — Stemming + Water + Emulsion

image[Figure 2: Hole 202 — Charging Summary]

Deck 1: INERT — Stemming .... 0.0 m to 3.0 m .... 3.0 m
Deck 2: INERT — Water ....... 3.0 m to 6.0 m .... 3.0 m
Deck 3: COUPLED — Emulsion .. 6.0 m to 13.8 m ... 7.8 m
Explosive mass: 390.3 kg

Calculations (using the full SDoB formula with M = 10 for 251 mm diameter):

SDoB(GEO)  = St=6.0m (all material above charge) → SDoB = 1.36  
           → Controlled Energy

SDoB(ADJ)  = St=4.5m (1.0 x 3.0 + 0.5 x 3.0) → SDoB = 1.08  
           → Controlled Energy

SDoB(IGN)  = St=3.0m (solid stemming only) → SDoB = 0.80  
           → Transitional

Here the three variants tell distinctly different stories. The geometric value places the hole at the upper end of controlled energy. The adjusted value recognises that water provides some confinement (hydrostatic pressure resists gas venting) but not as much as solid stemming, bringing the value down to 1.08. The ignored value — counting only the 3.0 m of solid stemming — drops the hole into the transitional range (0.80), flagging potential flyrock risk.

For flyrock risk assessment, the ignored value is the most relevant. For vibration prediction (where the water column does contribute to energy coupling into the ground), the adjusted value is more appropriate.

3.3 Hole 203 — Stemming Only + Emulsion (Baseline)

image[Figure 3: Hole 203 — Charging Summary]

Deck 1: INERT — Stemming .... 0.0 m to 3.6 m .... 3.6 m
Deck 2: COUPLED — Emulsion .. 3.6 m to 13.9 m ... 10.3 m
Explosive mass: 511.0 kg

Calculations (using the full SDoB formula with M = 10 for 251 mm diameter):

SDoB(GEO)  = St=3.6m  → SDoB = 0.92  
           → Controlled Energy (lower bound)

SDoB(ADJ)  = St=3.6m  → SDoB = 0.92  
           → Controlled Energy (lower bound)

SDoB(IGN)  = St=3.6m  → SDoB = 0.92  
           → Controlled Energy (lower bound)

When the entire column above the charge is solid stemming, all three variants converge to the same value. This is the baseline case and confirms that the framework introduces no distortion when air or water are absent. Note this hole sits right at the lower boundary of controlled energy (0.92), suggesting the stemming height is well matched to the charge.


4. Isometric Context View

The three holes shown above are displayed together in the Kirra 3D viewport, illustrating how different charging configurations appear in the context of the bench geometry.

image[Figure 4: 3D overview of Holes 201, 202, and 203]

image[Figure 5: Isometric view with Grade RL and Toe RL]

  • Hole 201 (pink, air deck) shows a visible gap between the stemming and the charge.

  • Hole 202 (teal/green, water) shows the water column transitioning to the emulsion.

  • Hole 203 (yellow, stemming only) shows a continuous column of stemming directly above the explosive.


5. Summary Comparison

Hole 201 — Stem + Air + ANFO
  SDoB(GEO): 1.43 | SDoB(ADJ): 1.05 | SDoB(IGN): 1.01
  → Air provides low but non-zero confinement

Hole 202 — Stem + Water + Emulsion
  SDoB(GEO): 1.36 | SDoB(ADJ): 1.08 | SDoB(IGN): 0.80
  → Water provides partial confinement; IGN flags transitional risk

Hole 203 — Stem + Emulsion (baseline)
  SDoB(GEO): 0.92 | SDoB(ADJ): 0.92 | SDoB(IGN): 0.92
  → All variants converge

6. Recommendations for Practice

  1. Always calculate all three variants when non-solid materials are present above the charge. The spread between them quantifies how much the column composition affects your confinement assessment.

  2. Use SDoB(GEO) for basic design compliance checks and pattern auditing, but be aware that it overstates confinement when air or water is present.

  3. Use SDoB(ADJ) for vibration and airblast prediction, where the partial confinement of water and the near-zero confinement of air need to be reflected in the energy partitioning model.

  4. Use SDoB(IGN) for flyrock risk assessment and exclusion zone determination. This is the most conservative variant and answers the question: "how much solid material is actually preventing crater-style venting?"

  5. Calibrate the confinement coefficients to your site conditions. The defaults in this note are reasonable starting points, but monitoring data (airblast, flyrock, vibration) should be used to refine them. In particular, the water coefficient can vary significantly depending on whether the water is static (groundwater) or dynamic (recently pumped/flowing).

  6. Report the variant used. When communicating SDoB values in blast reports, always specify which variant was calculated. An SDoB of 1.4 means very different things depending on whether it is geometric, adjusted, or ignored.


7. Implementation Notes

The three-variant framework is straightforward to implement in blast design software. The key requirement is that the charge plan data structure distinguishes between deck types — specifically, that each inert deck is tagged with its material type (stemming, air, water, drill cuttings, etc.) rather than being treated as a generic "non-explosive" segment.

In the Kirra blast design application (kirra-design.com), deck types are explicitly modelled with material properties including density, enabling automated calculation of all three SDoB variants from the charge plan. The upcoming blast-physics-js open-source library will expose these calculations as standalone functions.


References

  • Chiappetta, R.F. and Treleven, M.J. (1997). Scaled Depth of Burial. Blasting Analysis International, Inc. Allentown, PA, USA.

  • Chiappetta, R.F. (2010). Combining Electronic Detonators with Stem Charges and Air Decks. Drill and Blast 2010 Conference, Perth, Australia.

  • Department of the Army (1986). Fundamentals of Protective Design for Conventional Weapons. Technical Manual TM 5-855-1, Washington, DC, USA.

  • Drake, J.L. and Little, C.D. (1983). Ground Shock from Penetrating Conventional Weapons. Interaction of Non-Nuclear Munitions with Structures, US Air Force Academy.

  • Jhanwar, J.C. and Jethwa, J.L. (2000). The Use of Air Decks in Production Blasting in an Open Pit Coal Mine. Geotechnical and Geological Engineering, 18, pp. 269–287.

  • McKenzie, C., Blastechnology, Australia. Personal communication (email, November 2021) regarding SDoB formula correction, diameter-dependent M value capping, and the question of how air decks should be handled in SDoB calculations.

  • Sazid, M. and Singh, T.N. (2015). Numerical assessment of air-deck blasting. International Journal of Mining Science and Technology, 25(4), pp. 647–653.

  • Shelton, T.W. et al. (2014). Experimental and Numerical Investigation of the Ground Shock Coupling Factor for Near-Surface Detonations. Shock and Vibration, Article ID 789202.

  • Tobin, G. (2013). The Importance of Energy Confinement to the Blast Outcome & Justification for use of Stemming Plugs in Over Burden Removal. Oresome Products, Australia.


About

This technical note is published by Blasting Apps (blastingapps.com). The Kirra blast design application is available at kirra-design.com. Borehole cross-section figures were generated using Kirra.

For questions, corrections, or to share site calibration data for the confinement coefficients, contact Brent Buffham via blastingapps.com.

Figure List:

  • Figure 1 → hole201_air_deck.png

  • Figure 2 → hole202_water.png

  • Figure 3 → hole203_stemming_only.png

  • Figure 4 → kirra_3d_overview.png

  • Figure 5 → kirra_isometric_context.png


© 2026 Brent Buffham — Blasting Apps. All rights reserved.

Подобається цей допис?

Купити для BrentBuffham каву

Більше від BrentBuffham